If you’ve ever spent hours shaping a perfect ceramic mug, a delicate bowl, or a decorative vase only to pull it out of the kiln after the first firing and see your glaze slip, craze, or bubble over, you’re not alone. As a ceramic crafts supplier who’s worked with thousands of potters—from hobbyists testing their first glaze batch to small studios scaling up for retail—I’ve seen these mistakes derail more projects than I can count. Glaze is equal part science and art: it’s a layer of silica, fluxes, and metal oxides that melts to form a glassy, protective surface, and even tiny missteps in application, firing, or material prep can turn a flawless ceramic piece into something unusable. Today, I’m breaking down the most common glaze mistakes I see, why they happen, and actionable ways to avoid them, based on decades of working with makers and refining my own quality control processes for our supplier line. Ceramic Crafts

Mistake #1: Applying Glaze Too Thin or Too Thick
This is the most frequent error, and it’s easy to make when you’re rushing through a project. When you dip a piece, brush it on, or spray glaze, getting the right thickness (usually measured in thousandths of an inch, or mils, though most makers gauge by feel) is critical. Glaze that’s too thin will melt too much during firing, leaving the surface patchy, under-glazed, or even see-through in spots. I once received a batch of custom mugs from a small studio that had been dipped once instead of the recommended two times, and half the cups looked like they’d been dipped in water instead of glaze—light passed right through the handles, and the color was uneven, as if it had been wiped off in places. On the flip side, glaze that’s too thick can bubble, run, or crack as it dries, and during firing, it can cause “shivering” (when the glaze pulls away from the body like peeling paint) or even cause the piece to stick to the kiln shelf. I’ve had a decorative vase I made in a workshop days ago get rejected because the maker applied glaze so thickly to the base that it melted into a blob and fused to the shelf, ruining both the vase and the shelf.
How to avoid this? For dipping, I recommend two smooth, even dips, held for 2-3 seconds each, and wiping the base with a damp sponge immediately after to remove any excess glaze that would pool at the bottom. For brush application, use a stiff bristle brush and apply in thin, overlapping layers, waiting 15-20 minutes between coats so each layer can dry. If you spray glaze, use an air compressor set to 20-25 PSI, and hold the gun 6-8 inches away, moving in steady, horizontal passes—two thin coats are always better than one heavy one. A simple tool I swear by is a wet film gauge, which is a small plastic strip with notches that tells you exactly how thick your glaze is when applied; most craft stores carry them for under $10, and they eliminate guesswork.
Mistake #2: Not Prepping the Ceramic Body Before Glazing
You’d be surprised how many makers skip the prep step, thinking that once the piece is bisque-fired (the first low-temperature firing that hardens the clay), it’s ready for glaze. But a bisqueware piece still has dust, oils, and even tiny bits of clay residue on its surface that will interfere with glaze adhesion. If you don’t clean it properly, the glaze will “crawl” — pull away in small, round patches like a snake shedding skin — leaving bare spots where the clay body is exposed. I once had a client order 500 small planters, and 10% of them came back with crawling glaze; when we investigated, the studio had wiped the bisque pieces with a dry rag instead of a damp sponge, so there was loose kiln dust all over the surface. Even fingerprints from handling bisque can cause crawling, because the oils in your skin create a barrier between the clay and glaze.
Another part of prep is making sure the piece is fully dry before glazing. Glaze is a water-based mixture, and if the bisque is damp, the water in the glaze won’t absorb evenly. This can cause the glaze to bubble or blister during firing, as trapped water turns to steam and tries to escape through the glaze layer. I once made a bowl for a local craft fair that I thought was dry, but it had been sitting in a damp corner of my studio overnight. When I glazed it and put it in the kiln, a big blister popped on the side during the firing, leaving a rough, pitted spot that made the bowl unfit for sale.
How to avoid this? After bisque firing, let the pieces cool completely (usually 24 hours) before handling. Wipe the surface with a clean, damp sponge (not dripping wet) to remove all dust, then buff gently with a dry, lint-free cloth. For extra prep, many makers use a small brush to “biscuit wash” — a thin coat of water mixed with a tiny bit of china clay — which helps the glaze adhere better, especially to porous clay bodies like stoneware or earthenware. And always let bisque pieces dry for at least 48 hours after cleaning, or leave them in a low-humidity area for a few days, before glazing.
Mistake #3: Firing at the Wrong Temperature or Too Fast
Temperature is everything with glaze. Every glaze is formulated to melt at a specific range, called its “cone” — a measurement of heat in the kiln, where higher cone numbers mean higher temperatures. If you fire a low-temperature glaze (cone 05 to cone 04, good for earthenware) to a high stoneware temperature (cone 6), the glaze will become too fluid, run off the piece, and leave the body exposed. Conversely, firing a high-temperature glaze to too low a temperature means the glaze won’t melt properly, leaving a dull, powdery surface that’s not durable. I’ve seen this happen so many times with new makers: they use a glaze meant for stoneware but fire it in a kiln that only reaches cone 04, and the final product has a chalky finish that scratches off easily.
Firing speed is just as important as temperature. Rushing the kiln — cranking the heat up too quickly — causes two common issues: bubbling and carbon trapping. Bubbles happen when water or air in the glaze or clay body expands too fast and bursts before the glaze has a chance to settle. Carbon trapping occurs when the kiln is heated too quickly before the glaze has a chance to vitrify (become non-porous), and unburned organic matter from the clay burns and gets trapped under the glaze, leaving black or grey spots on the surface. I once had a client send a batch of mugs that had grey streaks inside; she’d fired the kiln in 8 hours instead of the recommended 12, so the organic material in the clay didn’t fully burn out and got stuck under the glaze on the inside of the mugs.
How to avoid this? First, always check the glaze’s recommended cone range before firing. Glaze containers (or our supplier product pages, for the many glazes we carry) list exactly what cone they’re designed for, so stick to that. Invest in a kiln sitter or a digital kiln controller, which takes the guesswork out of temperature and helps you maintain a consistent firing schedule. For bisque firing, ramp (increase heat) at 100-150 degrees per hour up to cone 06 or 05, then hold for 30 minutes to make sure all organic matter is burned out. For glaze firing, ramp at 150-200 degrees per hour up to the recommended cone, then hold for 15-30 minutes to let the glaze melt evenly and settle. If you’re using a manual kiln, mark your schedule on a calendar so you don’t rush — patience is half the battle here.
Mistake #4: Ignoring Glaze Compatibility or Thermal Shock
Glaze doesn’t exist in a vacuum — it has to work with your clay body, and even with other glazes if you’re layering colors. The most common issue here is thermal shock, which happens when the glaze and clay body expand and contract at different rates during cooling. This causes the glaze to craze — form fine, hairline cracks across the surface — which is more than just a cosmetic issue: crazing can make food or drink unsafe, as bacteria can get trapped in the cracks, and it can cause the glaze to chip off over time. I’ve seen dinner sets with crazed glaze that had to be recalled because they were unsafe for serving food, all because the studio used a glaze formulated for porcelain on a stoneware body, which has a higher thermal expansion rate.
Layering glazes adds another layer of complexity. If you apply a dark glaze over a light one without considering how they react chemically, you can get color bleeding, or even a muddy, dull finish. For example, if you apply a thin coat of blue glaze over white, but the blue glaze has a high amount of metallic oxides that leach into the underglaze during firing, the white will turn grey instead of staying bright. I once made a set of bowls with layered glazes for a local restaurant, and the blue overglaze made the white underglaze turn a dull taupe; I’d mixed two glazes with incompatible flux agents, which is why the color migrated.
How to avoid this? Always check that your glaze and clay body have matching thermal expansion rates. Most glaze suppliers (including us) list compatible clay bodies on product pages, or you can do a small test: make a tiny test tile from the same clay you’re using, apply the glaze, fire it, and see if it crazes when it cools. If it does, adjust the glaze composition (or switch to a glaze formulated for your clay) — there are guides online for small adjustments to thermal expansion. For layering glazes, do a test tile first: apply a thin coat of the underglaze, let it dry fully, apply the overglaze, fire it, and check the color. Wait 24 hours before making final pieces, to make sure the color doesn’t shift or bleed during cooling.
Mistake #5: Not Testing Glazes First
This is the mistake I see even experienced makers make: assuming a glaze will look the same as it does online, in a catalog, or on another type of clay. Glaze is sensitive to even small changes in materials, firing, and clay, so what works for one maker might not work for you. I once had a potter contact me in a panic because she ordered a glaze from a popular supplier that looked like a deep forest green in photos, but when she fired it, it turned a dull olive green with brown streaks. It turned out the glaze had a batch of metal oxide that was off, but also she was firing at a lower cone than recommended, and her clay body was more porous than the test tiles the supplier had used.
How to avoid this? Always do test firings before using a new glaze for a big order. Make small test tiles (3×3 inches works well) from the exact clay you’re going to use, apply the glaze the same way you will for your final pieces, and fire it according to the glaze’s instructions. If you’re layering, testing the layers is non-negotiable. Keep a glaze log: write down the glaze name, clay type, application method, firing cone, and how the final result turned out. This log becomes your reference for future projects, so you don’t have to guess each time. At our ceramic crafts supply company, we always tell new clients to order a sample kit first, which has small amounts of our most popular glazes and clay bodies, so they can test before committing to a large batch.
If you’re a maker looking to refine your glaze process, or a small business looking for reliable, consistent glaze materials to scale your ceramic crafts line, I’m here to help. We offer premium, test-approved glazes, clay bodies, and kiln accessories, plus free technical support for makers of all levels. Whether you’re making mugs, planters, decorative vases, or custom dinnerware, I can walk you through adjusting your glaze process to fit your specific needs and avoid the mistakes I outlined above.

To connect and discuss your project or order details, feel free to reach out for a no-obligation consultation.
Household Porcelain References
- Hamer, F., & Hamer, J. (2000). The Potter’s Dictionary of Materials and Techniques. A & C Black.
- Rhodes, D. (1973). Clay and Glazes for the Potter. Chilton Book Company.
- Tite, M. S. (1995). Ceramic Materials: Science and Technology. Woodhead Publishing.
- Wilson, E. (2018). Glaze Chemistry for Beginners. Lark Books.
Suixian Yaxin Porcelain Art Business Department (Individual Business)
With abundant experience, we are one of the most professional ceramic crafts manufacturers in China. Please feel free to buy top-quality ceramic crafts at competitive price from our factory. Welcome to contact us for pricelist and free sample.
Address: Yaxin Ciyu Ceramics Factory, Wenzhuang Village Committee, Hutang Township, Sui County, Shangqiu City, Henan Province
E-mail: 3602611251@qq.com
WebSite: https://www.xiangyiguyao.com/